dc.identifier.citationM.,John Paul; Prabavathy,S.: Investigation on flexural behavior of ferrocement slab with GGBS & nano silica. Timişoara: Editura Politehnica, 2019.en_US
dc.identifier.issn1582-4594-
dc.identifier.urihttps://dspace.upt.ro/xmlui/handle/123456789/7096-
dc.description.abstractThe flexural behavior of ferrocement slabs using GGBS & Nano Silica based geopolymer mortar are investigated experimentally. The geopolymer mortar for ferrocement slab is prepared as 1:2. The binder composed of 65% fly ash, 25% sodium silicate and 10% sodium hydroxide. The percentage of fly ash is altered by using GGBS as 20%, 40%, 60%, 80% & 100% by its weight. Even though the optimum strength obtained with 100% fly ash by GGBS, 80% of GGBS addition is taken due to the early formation of cracks at 100% of GGBS addition. The performance of the selected mix is further improved by adding Nano Silica as 0.5%, 1%, 1.5% & 2% by weight of binder. With the 1.5% of Nano Silica and 80% of GGBS, the geopolymer mortar acquired over 250% increase in strength.en_US
dc.language.isoenen_US
dc.publisherTimișoara : Editura Politehnicaen_US
dc.relation.ispartofseriesJournal of Electrical Engineering;Vol 19 No 2-
dc.subjectGeopolymer mortaren_US
dc.subjectGGBSen_US
dc.subjectNano-silicaen_US
dc.subjectFerrocementen_US
dc.subjectSlabsen_US
dc.titleInvestigation on flexural behavior of ferrocement slab with GGBS & nano silica [articol]en_US
dc.typeArticleen_US
Appears in Collections:Articole științifice/Scientific articles

Files in This Item:
File Description SizeFormat 
BUPT_ART_Paul_f.pdf625.4 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.