Please use this identifier to cite or link to this item: https://dspace.upt.ro/xmlui/handle/123456789/7096
Title: Investigation on flexural behavior of ferrocement slab with GGBS & nano silica [articol]
Authors: M., John Paul
Prabavathy, S.
Subjects: Geopolymer mortar
GGBS
Nano-silica
Ferrocement
Slabs
Issue Date: 2019
Publisher: Timișoara : Editura Politehnica
Citation: M.,John Paul; Prabavathy,S.: Investigation on flexural behavior of ferrocement slab with GGBS & nano silica. Timişoara: Editura Politehnica, 2019.
Series/Report no.: Journal of Electrical Engineering;Vol 19 No 2
Abstract: The flexural behavior of ferrocement slabs using GGBS & Nano Silica based geopolymer mortar are investigated experimentally. The geopolymer mortar for ferrocement slab is prepared as 1:2. The binder composed of 65% fly ash, 25% sodium silicate and 10% sodium hydroxide. The percentage of fly ash is altered by using GGBS as 20%, 40%, 60%, 80% & 100% by its weight. Even though the optimum strength obtained with 100% fly ash by GGBS, 80% of GGBS addition is taken due to the early formation of cracks at 100% of GGBS addition. The performance of the selected mix is further improved by adding Nano Silica as 0.5%, 1%, 1.5% & 2% by weight of binder. With the 1.5% of Nano Silica and 80% of GGBS, the geopolymer mortar acquired over 250% increase in strength.
URI: https://dspace.upt.ro/xmlui/handle/123456789/7096
ISSN: 1582-4594
Appears in Collections:Articole științifice/Scientific articles

Files in This Item:
File Description SizeFormat 
BUPT_ART_Paul_f.pdf625.4 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.